What should the melt pool look like?
Updated
On this page8
In a well-wicked container candle, the melt pool (the layer of liquid wax around the wick) spreads to the wall or very close to it within three to four hours of burning, stays a modest depth, and leaves no ring of hard wax on the glass once the first few burns are behind it. That is the practice figure candle suppliers publish, and it is practice: no ASTM standard or retailer protocol sets a melt pool target. This page gives the suppliers' figures side by side, shows how to measure width and depth, and explains what a slow, fast, shallow or deep pool says about the wick.
What suppliers say a good pool looks like
These are each supplier's published guidance for its own waxes and wicks. They broadly agree on timing and differ on depth.
| Supplier | Width and timing | Depth | Notes |
|---|---|---|---|
| CandleScience [1] | No more than 1/4 inch (6 mm) from the edge of the container at three to four hours | About 1/4 to 1/2 inch (6 to 13 mm), slight variance acceptable | Wax left on the wall should melt down by the third or fourth cycle; do not judge the pool critically until four or more cycles |
| Supplies for Candles (UK) [2] | Full melt pool by hour 3 to 4; wick up if it has not reached the edge by then | No figure; wick down if the pool is too deep | Test at least three wick sizes |
| Northwood [3] | No time given | Between 1/4 and 3/4 inch when fully melted | Record pool size and depth at regular intervals, for example hourly |
| Makesy, for wood wicks [4] | Full diameter at 2 hours; to the vessel edge at 4 hours | 1/2 inch (12.7 mm) at 4 hours | Wood wick figures only; deeper than 1/2 inch means the wick is too big |
Two things follow from the table. First, "three to four hours" is the common timing for cotton wicks in container wax, and a wood wick is expected to move faster. Second, the depth figures overlap but do not match: CandleScience's upper figure of 1/2 inch is Northwood's middle. This page uses CandleScience's 1/4 to 1/2 inch as the working range because it comes with a timing and a cycle count, and treats anything deeper as a sign to look hard at flame height and vessel temperature. If your wax maker publishes its own figure, use that.
Retail protocols do not set a melt pool target either. Kohl's Test Protocol 100-Z (February 2025), the most complete published one, checks overflow (molten wax must not escape and reach the surface the candle sits on), but sets no width or depth [5].
How to measure the pool
Width. At each hourly reading, look straight down and estimate how far the liquid edge is from the wall, in millimeters or fractions of an inch. A photo from directly above with a ruler laid across the rim gives you a record you can measure later. Note whether the pool is even around the wick or lopsided.
Depth. Dip a wooden skewer or toothpick straight down beside the wick, not touching it, until it meets solid wax. Lift it out and measure the wet part. Do this at the same hourly readings so you can see the trend.
Wall wax. After the candle cools, look at the side of the jar. A ring of unmelted wax clinging to the glass above the surface is "hang-up." A little after the first one or two burns is expected; CandleScience says it should be gone by the third or fourth cycle [1].
Time to full pool. Write down the hour at which the pool first reaches the wall (or comes within your target distance). This is the single most useful number for comparing wick sizes in the same jar.
What the pool is telling you
| What you see | What it usually means | What to do |
|---|---|---|
| Pool well short of the wall at 4 hours, still short after the fourth cycle | The wick is too small for this diameter, wax and load. CandleScience treats unmelted wax at the edge after the fourth cycle as a sign you may need to wick up [1] | Test the next wick size up; see when to change the wick size |
| A narrow hole forming down the center | Tunneling, the long-term result of a pool that never reaches the wall | Why candles tunnel |
| Pool reaches the wall in an hour or two (cotton wick) | Far more fuel than the jar needs; the flame is often tall and the jar hot | Check flame and vessel temperature, then test a size down |
| Pool deeper than your working range | Over-wicked, or wax that melts very easily. Supplies for Candles and Makesy both say a too-deep pool means wick down [2] [4] | Measure flame and jar temperature; test a size down |
| Pool full at 3 to 4 hours, depth in range, no hang-up after cycle 4 | A wick that suits this build | Keep testing to the end of the candle before deciding |
| Pool lopsided, deeper on one side | Wick off center, leaning, or a draft | Check wick centering and the room; see attaching and centering wicks |
| Flame shrinks and goes out as the pool deepens | The wick is drowning in its own pool | A candle that keeps going out |
| Wax runs over the rim | Overflow, a failure in the Kohl's protocol [5] | Stop the burn; the wick is too large or the fill too high |
Why the same wick pools differently in different waxes
A wick chart is built on one set of assumptions. CandleScience's wick recommendations assume a 7.5 percent fragrance load and no dye, and it notes that dyed or heavily fragranced candles may need a larger wick [6].
Wax viscosity matters as much. CandleScience reports that its coconut apricot wax has a lower viscosity when liquid than pure soy, so it travels up the wick faster and generally needs a smaller wick than soy to avoid feeding the flame too much fuel [7]. The same wick that gives a slow pool in a firm soy container wax may give a deep, fast pool in a softer blend. CandleScience also says beeswax is harder to predict and will take more testing to find the right wick [6].
So when you change wax, load or dye, the melt pool is the first thing that will move. What has to be retested covers which of those changes need a full test.
The first burns and the memory a candle keeps
Makers often say a container candle "remembers" its first pool, and that a short first burn sets up tunneling. None of the suppliers cited here gives a figure for that, so treat it as a description of what you will see rather than a rule. What the sources do say is consistent: judge the pool over several full sessions. CandleScience says not to draw conclusions until at least the fourth burn cycle [1], and Supplies for Candles warns against testing before the candle is fully cured, because early tests give misleading results [2]. A pool that is short on burn one and full by burn three is a different result from one that is short every time. Your records should show which you have.
Multi-wick pools
In a candle with two or three wicks, each wick melts its own pool and the pools should merge into one. Watch for pools that join early and then deepen fast, which means the wicks are heating each other and the vessel. When a candle needs two or three wicks explains how suppliers size each wick.
Reading the pool alongside the flame
The pool and the flame move together. A deep pool with a tall flame points to an oversized wick; a shallow pool with a small, steady flame points to an undersized one. Measure both at every hourly reading, using measuring flame height for the method, then take both readings to when to change the wick size to decide which way to move.
Top picks
Top containers for candles
4 oz · 58-400 · Glass · Amber · 2.6 in
16 oz · 89-400 · Glass
9 oz · 70-400 · Glass
4 oz · 58-400 · Glass · Clear
4 oz · 58-400 · Glass · Amber · 2.7 in
6 oz · 63-400 · Glass
4 oz · Steel
12 oz · 63-400 · Glass
References
- CandleScience, How to Conduct a Burn Test, undated, read October 22, 2026. https://candlescience.com/learning/how-to-conduct-a-burn-test/
- Supplies for Candles, The Complete Guide to Wick Testing: What Every Candle Maker Needs to Know, published February 26, 2026, modified September 2, 2026. https://www.suppliesforcandles.co.uk/the-complete-guide-to-wick-testing-what-every-candle-maker-needs-to-know/
- Northwood, How to Test Candles (help center article), undated, read October 22, 2026. https://northwood-knowledge.groovehq.com/help/how-to-test-candles
- Makesy, Candle Burn Testing 101, October 28, 2020. https://makesy.com/blogs/news/candle-burn-testing-101
- Kohl's, Private Brands Performance Claims Test Protocols 100, Protocol 100-Z: Candle (including freestanding, taper, tealight, votive, filled and novelty candles), revised February 2025 (current revision; candle limits unchanged from 100-Y, February 2023), read October 22, 2026. https://link.kohls.com/content/dam/klink/100-Z-CANDLE.pdf
- CandleScience, Candle Wick (wick category page and recommendations), undated, read October 22, 2026. https://www.candlescience.com/candle-wick
- CandleScience, Lab Notes: CandleScience Coconut Apricot Wax, undated (images dated April 2024), read October 22, 2026. https://candlescience.com/lab-notes-candlescience-coconut-apricot-wax