It cured cloudy, or it never cured
Updated
On this page11
The inclusion was not dry
A dried flower or a botanical holding moisture clouds the resin around it and sometimes blooms. A lined closure and a desiccant is the whole fix.
The mold had dust on it
Invisible until the casting comes out. Silicone attracts dust and an open shelf is an invitation; a closed container is the only reliable answer.
The mold had taken a set
Stored creased or under weight. The casting comes out with a shape nobody designed and the mold does not recover.
The pigment attacked the bottle
An alcohol ink in PET. The wall clouds or softens, the ink picks up whatever leached, and the color shifts. 130 glass containers here exist for this.
The colorant evaporated
A solvent-borne dye through a poor liner. The remaining ink is stronger than it was, which ruins color repeatability before it ruins the ink.
The mica caked
Moisture into a powder with a loose cap. It can be broken up and it will never disperse the same way, which shows as streaks in a casting.
The glitter went everywhere
Static and a narrow mouth. A spill of fine flake contaminates every other color on the bench, which is why glitter wants individual sealed containers more than any other material here.
The findings got mixed
Certified and uncertified parts in one tray. For a maker running a children's line that is a compliance failure with no way to unpick it after the fact.
Which is the batch record argument again
Cohort information is only as good as knowing what went into the pour. Separate, labeled storage is what makes the mark on the package mean something.
Test the storage, not the resin
Put a mold, a dried flower and a filled pigment bottle away for three months, then use them. Every failure on this page shows up in that test and none of them show up on the day you fill.